Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) <= 20 ppm
<= 20 ppm
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a..
Ionic Impurities - Na (Sodium) <= 20 ppm
<= 20 ppm
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a..
Ionic Impurities - Na (Sodium) <= 20 ppm
<= 20 ppm
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca..
Ionic Impurities - Na (Sodium) <= 20 ppm
<= 20 ppm
Ferro IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: TF Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can..
Copyright © lookpolymers.com All Rights Reserved