Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 13 ppm
13 ppm
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..