Polymer Property : Critical Temperature = 924 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 924 °C
1700 °F
Ac3
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service ..