Polymer Property : Critical Temperature = 823 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 823 °C
1510 °F
Ac3
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1)
TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load..