Polymer Property : Critical Temperature = 802 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 802 °C
1480 °F
Ac1
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420)
TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an..
Critical Temperature 802 °C
1480 °F
Ac1
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420)
TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu..
Critical Temperature 802 °C
1480 °F
Ar1
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel
TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications...
Critical Temperature 802 °C
1480 °F
Ar1
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13)
TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu..
Critical Temperature 802 °C
1480 °F
Ar1
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S)
Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi..
Critical Temperature 802 °C
1480 °F
Case Ac3
Latrobe CBS-600â„¢ VIM-VAR Carburizing Bearing and Gear Steel
CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe..