Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 78.4 °C | 173 °F | |
Solvay Specialty Polymers Meforex® 32 Ozone-Friendly CFC Replacement Formula: CH2F2; Name: Difluoromethane. Replaces R 502, R22. Refrigerant blends component.Information provided by Solvay Solexis, Inc. |