Chemical Properties Metric English Comments
Critical Temperature 774 °C
1430 °F
Ar3
Latrobe TNWâ„¢ ASTM M10 High Speed Steel
TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2% vanadium content. TNW is popul..
Critical Temperature 774 °C
1430 °F
Ar1
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1)
TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load..