Polymer Property : Critical Temperature = 763 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 763 °C
1410 °F
Ac1
Latrobe LSS™ P20 Mold Steel (ASTM P20)
TLS P20 mold steel is a versatile, low-alloy tool steel that is characterized by good toughness at moderate strength levels. The steel is commonly used for plastic injection mold cavities and toolin..