Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 751.7 °C | 1385 °F | |
Crucible Steel AISI 52100 Alloy Steel Information provided by Crucible Industries |
|||
Critical Temperature | 751.7 °C | 1385 °F | |
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |