Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 740 °C | 1360 °F | Ac1 |
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |