Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 624 °C | 1160 °F | Ac1 |
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide s.. |
|||
Critical Temperature | 624 °C | 1160 °F | Ac1 |
Latrobe Lescalloy® HY-180 VIM-VAR ; 2.01 - 4.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |
|||
Critical Temperature | 624 °C | 1160 °F | Ac1 |
Latrobe Lescalloy® HY-180 VIM-VAR ; 4.01 - 8.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |