Chemical Properties Metric English Comments
Critical Temperature 168 °C
334 °F
Martensitic Finish
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Critical Temperature 168 °C
334 °F
Martensitic Finish
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Critical Temperature 168 °C
334 °F
Martensitic Finish
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Critical Temperature 168 °C
334 °F
Martensitic Finish
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..