Chemical Properties Metric English Comments
Critical Temperature 86.0 °C
187 °F
Shandong Dongyue Shenzhou New Material Co Hexafluoropropene Oxide (HFPO)
Conformable with: Q/DYS 002-2007Hexafluoropropene Oxide (HFPO) is a kind of colorless and uninflammable gas. It is easy to be liquefied under pressure, and generally be used as special intermediate..