Chemical Properties Metric English Comments
Critical Temperature 877 °C
1610 °F
Ac3
Latrobe Double Six™ ASTM M2 High Speed Steel
DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far the most popular high speed ..