Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 835.0 °C | 1535 °F | |
Crucible Steel CHRO-MOW® Tool Steel, AISI H12 Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar.. |
|||
Critical Temperature | 835.0 °C | 1535 °F | |
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |