Critical Temperature 719 °C
1330 °F
Ac1
Latrobe LSS™ L6 Tool Steel (ASTM L6)
TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good ..