Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 703 °C | 1300 °F | Ar1 |
Latrobe LSS™ O1 Tool Steel (ASTM O1) TLS O1 tool steel is the original oil-hardening, "non-shrinking" tool steel that can be hardened to the Rockwell C 65 range from a low austenitizing temperature. TLS O1 is a general-purpose tool ste.. |