Polymer Property : Linear Mold Shrinkage, Flow = 0.0135 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0135 cm/cm

@Time 86400 sec
0.0135 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY M3000 PP
LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat.