Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0108 cm/cm @Time 86400 sec |
0.0108 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0108 cm/cm @Time 86400 sec |
0.0108 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Linear Mold Shrinkage, Flow | 0.0108 cm/cm @Time 86400 sec |
0.0108 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |