Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0099 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0099 cm/cm

@Time 86400 sec
0.0099 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Linear Mold Shrinkage, Flow 0.0099 cm/cm

@Time 86400 sec
0.0099 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..