Polymer Property : Linear Mold Shrinkage, Flow = 0.0082 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0082 cm/cm

@Time 86400 sec
0.0082 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0082 cm/cm

@Time 86400 sec
0.0082 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific)
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region.