Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS
LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific)
LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.