Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific)
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer
LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific)
LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0073 cm/cm

@Time 86400 sec
0.0073 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.