Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific)
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC
LNP* THERMOCOMP* DB008ERP is a compound based on Polycarbonate resin containing 40% Glass Bead. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Flow 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific)
LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Flow 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Copyright © lookpolymers.com All Rights Reserved