Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP KONDUIT OTF2B PPS - Linear
LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Linear Mold Shrinkage, Flow 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS
LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing.