Physical Properties | Metric | English | Comments |
---|---|---|---|
Solubility | 8.0 ppm | 8.0 ppm | |
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |