Physical Properties Metric English Comments
Vapor Pressure 0.0124 bar

@Temperature 204 °C
9.27 torr

@Temperature 400 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..