Physical Properties Metric English Comments
Vapor Pressure 5.33e-10 bar

@Temperature 40.0 °C
4.00e-7 torr

@Temperature 104 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..