Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.52676 bar @Temperature 288 °C |
395.10 torr @Temperature 550 °F |
|
Duratherm LT Paraffinic Heat Transfer Fluid Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat.. |