Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0430 bar @Temperature 0.000 °C |
32.3 torr @Temperature 32.0 °F |
Concentration 0.36 kg HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (31 wt% - 36 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |