Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.002668 bar @Temperature 232 °C |
2.001 torr @Temperature 450 °F |
|
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |