Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000669 bar @Temperature 204 °C |
0.502 torr @Temperature 400 °F |
|
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |