Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000213 bar @Temperature 25.0 °C |
0.160 torr @Temperature 77.0 °F |
|
Dow Hydroxypropyl Acrylate Hydroxypropyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow |