Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | <= 0.0000267 bar @Temperature 50.0 °C |
<= 0.0200 torr @Temperature 122 °F |
AboCure |
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Vapor Pressure | <= 0.0000267 bar @Temperature 50.0 °C |
<= 0.0200 torr @Temperature 122 °F |
AboCure |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |