Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | <= 57 cSt @Temperature 100 °C |
<= 57 cSt @Temperature 212 °F |
|
Unipetrol R2 Heavy Fuel Oil Heavy fuel oil R2 is a mixture of mostly higher hydrocarbons obtained from crude oil through distillation and other refining processes. It may contain additives to lower its freezing point, or addit.. |