Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 410 cSt @Temperature 37.8 °C |
410 cSt @Temperature 100 °F |
|
Dow VORANOL™ 4240 Polyether Polyol VORANOL™ 4240 polyether polyol is a nominal 4000 molecular weight diol based on propylene oxide with ethylene oxide capping. Its high molecular weight and enhanced reactivity make it well suited t.. |