Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1950 cSt @Temperature -54.0 °C |
1950 cSt @Temperature -65.2 °F |
Kinematic Viscosity; ASTM D445 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Viscosity Measure | 1950 cSt @Temperature -54.0 °C |
1950 cSt @Temperature -65.2 °F |
Kinematic Viscosity; ASTM D445 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Viscosity Measure | 1950 cSt @Temperature -54.0 °C |
1950 cSt @Temperature -65.2 °F |
Kinematic Viscosity; ASTM D445 |
ExxonMobil Mobil Aero HF Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Viscosity Measure | 1950 cSt @Temperature -54.0 °C |
1950 cSt @Temperature -65.2 °F |
Kinematic Viscosity; ASTM D445 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |