Physical Properties Metric English Comments
Viscosity Measure 10495 cSt

@Temperature -51.0 °C
10495 cSt

@Temperature -59.8 °F
Kinematic Viscosity after 72 hr
ExxonMobil Mobil Avrex S Turbo 256
Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combination provides outstanding thermal and oxid..
Viscosity Measure 10495 cSt

@Temperature -51.0 °C
10495 cSt

@Temperature -59.8 °F
Kinematic Viscosity after 72 hr
ExxonMobil Mobil Avrex S Turbo 256
Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combination provides outstanding thermal and oxid..