Polymer Property : Viscosity Measure = 10 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure <= 10 cSt

@Temperature 150 °C
<= 10 cSt

@Temperature 302 °F
Unipetrol R2 Heavy Fuel Oil
Heavy fuel oil R2 is a mixture of mostly higher hydrocarbons obtained from crude oil through distillation and other refining processes. It may contain additives to lower its freezing point, or addit..