Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity Measure = 0.30 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Measure 0.30 cSt

@Temperature 232 °C
0.30 cSt

@Temperature 450 °F
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..