Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.65 g/cc @Temperature 600 °C |
0.276 lb/in³ @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Density | 7.65 g/cc @Temperature 600 °C |
0.276 lb/in³ @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |