Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.98 g/cc @Temperature -54.0 °C |
0.0715 lb/in³ @Temperature -65.2 °F |
|
Solvay Specialty Polymers Galden® D05 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |