Density 1.77 g/cc

@Temperature 25.0 °C
0.0639 lb/in³

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® D02 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Density 1.77 g/cc

@Temperature 25.0 °C
0.0639 lb/in³

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® D02TS PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..