Physical Properties Metric English Comments
Density 1.23 g/cc

@Temperature 25.0 °C
0.0444 lb/in³

@Temperature 77.0 °F
Solid
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing..