Polymer Property : Density = 1.095 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.095 - 1.124 g/cc

@Temperature 20.0 °C
0.03956 - 0.04061 lb/in³

@Temperature 68.0 °F
A Grade
Kazanorgsintez Triethanolamine
Production Method: Grades A and B are obtained by ammonia oxyethylation, Grade 'Clarified' is achieved by purified monoethanolamine oxyethylation. Application: Industrial triethanolamine is the comp..
Density 1.095 - 1.135 g/cc

@Temperature 20.0 °C
0.03956 - 0.04100 lb/in³

@Temperature 68.0 °F
"Clarified" Grade, B Grade
Kazanorgsintez Triethanolamine
Production Method: Grades A and B are obtained by ammonia oxyethylation, Grade 'Clarified' is achieved by purified monoethanolamine oxyethylation. Application: Industrial triethanolamine is the comp..