Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.996 g/cc @Temperature 45.0 °C |
0.0360 lb/in³ @Temperature 113 °F |
|
BASF Pluracol® 1135i Specialty Polyol Description: Pluracol® 1135i polyol is a nominal 1500 molecular weight triol. Pluracol 1135i has been prepared for applications in flexible slabstock foams and polyurethane adhesive and sealants ap.. |
|||
Density | 0.996 g/cc @Temperature 32.2 °C |
0.0360 lb/in³ @Temperature 90.0 °F |
|
BASF Pluracol® 858 Specialty Polyol Description: Pluracol® 858 polyol is a modifying polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elast.. |
|||
Density | 0.996 g/cc @Temperature 37.8 °C |
0.0360 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® P1010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |