Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.952 - 0.958 g/cc @Temperature 20.0 °C |
0.0344 - 0.0346 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT75-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |