Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9334 g/cc @Pressure 0.0481 MPa, Temperature 25.0 °C |
0.03372 lb/in³ @Pressure 6.98 psi, Temperature 77.0 °F |
|
Solvay Chemicals Allyl chloride 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.9334 g/cc @Pressure 0.0481 MPa, Temperature 25.0 °C |
0.03372 lb/in³ @Pressure 6.98 psi, Temperature 77.0 °F |
|
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |
|||
Density | 0.9334 g/cc @Pressure 0.0481 MPa, Temperature 25.0 °C |
0.03372 lb/in³ @Pressure 6.98 psi, Temperature 77.0 °F |
|
Solvay Chemicals Allyl chloride High purity 3-chloropropene Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6.. |