Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.887 g/cc @Temperature -45.6 °C |
0.0320 lb/in³ @Temperature -50.0 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |