Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.836 g/cc @Temperature 37.8 °C |
0.0302 lb/in³ @Temperature 100 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |